VAK Russia 05.02.2007 UDC 53 CSCSTI 20.01 VAK Russia 05.02.2013 CSCSTI 20.15 CSCSTI 20.17 CSCSTI 20.19 CSCSTI 55.01 CSCSTI 55.03 CSCSTI 55.13 CSCSTI 55.15 CSCSTI 55.16 CSCSTI 55.18 CSCSTI 55.19 CSCSTI 55.20 CSCSTI 55.21 CSCSTI 55.22 CSCSTI 55.23 CSCSTI 55.24 CSCSTI 55.29 CSCSTI 55.30 CSCSTI 55.31 CSCSTI 55.33 CSCSTI 55.35 CSCSTI 55.37 CSCSTI 55.41 CSCSTI 55.42 CSCSTI 55.43 CSCSTI 55.45 CSCSTI 55.47 CSCSTI 55.51 CSCSTI 55.53 CSCSTI 55.55 CSCSTI 55.57 CSCSTI 55.69 CSCSTI 73.01 CSCSTI 73.29 CSCSTI 73.31 CSCSTI 73.39 CSCSTI 73.41

SIMULATION OF METAL TRANSFER BETWEEN CYLINDRICAL ELECTRODES AT ELECTROSPARK ALLOYING

Published in Bulletin of Bryansk state technical university · Issue 8, 2019 · Pages 49–55 · Rubric: Mechanical engineering
DOI: https://doi.org/10.30987/article_5d6cbe42af6c79.15380930
Received: 29.08.2019 Accepted: 29.08.2019 Published: 29.08.2019 Language of publication: ru-RU
The work is dedicated to the simulation of the processes of erosion and electrode metal transfer at coating formation by an electrospark alloying method. Anode is a cylindrical rod, and cathode – a disk. During discharge pulses the erosion takes place both in anode material, and in cathode material. The anode moves in a spiral along a cathode surface. There are calculated the coefficients of precipitation equal to the probability of metal emitted from the surface of one electrode and falling onto the surface of the opposite electrode. They are constant close to the central cathode axis, but at the anode approach to the cathode end a coefficient of anode metal precipitation on a cathode decreases, a coefficient of cathode metal precipitation on an anode increases. The rates of anode erosion and cathode weight increase when the mass ratio of eroded substance of anode and cathode increases in the course of one discharge. When this ratio is equal to 5, a coefficient of mass transfer achieves 0.8-0.9 it tells of small substance loss during its transfer between electrodes. The model developed is useful for the parameter estimate of mass transfer between cylindrical electrodes at electrospark processing taking into ac-count their dimensions and paths of anode motion.
electric discharge, electrospark alloying, electrodes, precipitation, coefficient of mass transfer
Text References
Text (PDF)
Read Download

1. Verhoturov, A.D. Formirovanie poverhnostnogo sloya metallov pri elektroiskrovom legirovanii / A.D. Verhoturov. - Vladivostok: Dal'-nauka, 1995. - 282 s.

2. Wang, B.-J. Spark erosion behavior of silver-based particulate composites / B.-J. Wang, N. Saka // Wear. - 1996. - V. 195. - R. 133-147.

3. Ekmekci, B. White layer composition, heat treatment and crack formation in electric discharge machining process / B. Ekmekci // Metal. Mater, Trans. B. - 2009. - V. 40. - R. 70-81.

4. Chen, Z. Surface modiication of resistance welding electrode by electro-spark deposited composite coatings. Part I. Coating characterization / Z. Chen, Y. Zhou // Surf. Coat. Technol. - 2006. - V. 201. - R. 1503-1510.

5. Namitokov, K.K. Elektroerozionnye yavleniya / K.K. Namitokov. - M.: Energiya, 1978. - 456 s.

6. Galinov, I.V. Mass transfer trends during electrospark alloying / I.V. Galinov, R.B. Luban // Surf. Coat. Technol. - 1996. - V. 79. - R. 9-18.

7. Frangini, S. A study on the efect of a dy-k-l-h -h-k-Z-namic contact force control for improving electrospark coating properties / S. Frangini, A. Masci // Surf. Coat. Technol. - 2009. - V. 204. - Is. 16-17. - R. 2613-2623.

8. Pyachin, S.A. O zavisimosti izmeneniya massy elektrodov ot vremeni pri elektroiskrovom legirovanii / S.A. Pyachin, N.E. Ablesimov, D.L. Yagodzinskiy // Elektronnaya obrabotka materialov. - 2003. - № 1. - S. 19-26.

9. Sharakhovsky, L. Model of workpiece erosion for electrical discharge machining process / L. Sharakhovsky, A. Marotta, A.M. Essiptchouk // Appl. Surf. Sci. - 2006. - V. 253. - R. 797-804.

10. Pyachin, S.A. Vliyanie razmerov i raspolozheniya elektrodov na perenos metallov pri elektroiskrovom legirovanii / S.A. Pyachin // Fizika i himiya obrabotki materialov. - 2017. - № 1. - S. 17-28.